Diamond-cBN Alloy Bulk Samples and Diamond-cBN Alloy Cutters. (IMAGE)
Caption
A and B show a bulk diamond-cBN alloy samples synthesized at 20 GPa/2200 °C with a diameter of ~3 mm, over a copper screen to exhibit its transparency C and D show polished rake faces of diamond-cBN alloy cutters.