Figure 2 (IMAGE)
Caption
Crystal structural evolution of Mg4C60 within Li+ insertion/extraction. a In situ SXPD patterns of the Mg4C60 electrode during discharge/charge process with b corresponding galvanostatic charge/discharge profiles, d spacing variations, and intensity changes of broad peaks at ~21°. c 13C MAS-SSNMR spectra of pristine C60, Mg4C60, Mg4C60 after first discharge (Mg4C60-1D) and first full cycle (Mg4C60-1C). d AIMD simulation results of Mg4C60 with 12 inserted Li+ ions at original status and after various simulation steps.
Credit
©Shijian Wang et al.
Usage Restrictions
Reporters may freely use these materials in news coverage with appropriate credit information.
License
Licensed content