Before and After Charge-discharge (IMAGE)
Caption
Transmission electron microscopy reveals the new conducting polymer’s improved binding properties. At left, silicon particles embedded in the binder are shown before cycling through charges and discharges (closer view at bottom). At right, after 32 charge-discharge cycles, the polymer is still tightly bound to the silicon particles, showing why the energy capacity of the new anodes remains much higher than graphite anodes after more than 650 charge-discharge cycles during testing.
Credit
Lawrence Berkeley National Laboratory
Usage Restrictions
None
License
Licensed content